I've only had my A10T for a few weeks. When I first got it I had very bad stringing, like you are having and a week later, everything worked better.
https://i.imgur.com/VrwO4Z6.jpg
My speed is 60mm/s, retraction 6mm and retraction speed 40mm/s, and added a coast distance of .1mm and running at 205c. I'm running hot because I'm mixing soluble filament which likes a hotter temp with pla. My fan speed is 60%, with jumps at 100%. .4mm nozzle height, .4mm nozzle, .2mm layer height.
I also reseated the white tubes going from the feed to the extruder.
I have not changed the nozzle. The filament in the photo is the same brand as used i the video, so I do not credit filament. The blue filament in the video is one from geetech and the other are hatchbox, which I haven't noticed a difference.
Still a work in progress.
https://i.imgur.com/MBYilfI.mp4